Heat conduction Q1, convective heat transfer Q2 and radiation heat transfer Q3. Heat conduction refers to the heat transfer between objects in contact with each other through the thermal movement of free electrons, molecules, atoms and other microscopic particles. Convection heat transfer refers to the relative displacement between fluids, causing the mutual penetration of hot and cold fluids to achieve heat transfer. Radiation heat transfer is It refers to the temperature of the object itself that emits electromagnetic waves or photons to transfer heat.

 

insulation high alumina bricks

 

Generally, thermal insulation materials are multi-phase materials, and each phase has its own unique structure. Therefore, the thermal conductivity of thermal insulating refractory bricks is affected by many factors such as the composition, content, and internal structure of the phases. Therefore, there are many thermal insulation mechanisms and factors that affect its thermal insulation effect. The thermal conductivity of the thermal insulation material interacts with the bulk density, porosity, phase composition, etc. of the material.

 

(1)Stomata size:


(2)Bulk density:


(3) Material components:
The emissivity of thermal insulation materials is related to the material, temperature and particle size. Therefore, the ratio of thermal insulation materials can be appropriately increased or components with low emissivity such as Al2O3, MgO, CaO, and ZnO can be added, while Fe, Ni, and Cr should be avoided. Incorporation of transition element oxides.
​

Lähetä kysely

whatsapp

Puhelin

Sähköposti

Tutkimus